1-20 of 17966
Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Image
Design-print-test workflow. a/b Design of uniform (left) and density graded...
Published Online: October 5, 2022
Fig. 1 Design-print-test workflow. a/b Design of uniform (left) and density graded (right): ( a ) BCC and ( b ) SP lattices composed of an array of 6 × 6 × 6 unit cells. ( c ) Slicing and ( d ) printing steps with short-fiber-reinforced polymer. ( e ) Quasi-static compression testing. More
Image
( a ) and ( c ) Uniform ( ρ  = 0.35) and ( b ) and ( d ) graded ( ρ  = [0.2...
Published Online: October 5, 2022
Fig. 2 ( a ) and ( c ) Uniform ( ρ = 0.35) and ( b ) and ( d ) graded ( ρ = [0.2–0.8]) lattices comprised of tessellated ( a ) and ( b ) BCC and ( c ) and ( d ) SP unit cells ready for testing More
Image
Illustration of measurements on the uniform SP lattice with  ρ  = 0.2 and t...
Published Online: October 5, 2022
Fig. 3 Illustration of measurements on the uniform SP lattice with ρ = 0.2 and their post-processing. ( a ) True stress versus elastic or plastic true strain. ( b ) Transverse strain versus axial strain curve used to obtain the elastic Poisson’s ratio. More
Image
Non-dimensional plastic foam hardening characteristics for various lattice ...
Published Online: October 5, 2022
Fig. 4 Non-dimensional plastic foam hardening characteristics for various lattice densities of the ( a ) BCC and ( b ) SP lattice. The flow stress is normalized by the initial yield stress. More
Image
Image
Image
Comparison between the simulated and measured true stress–strain data of th...
Published Online: October 5, 2022
Fig. 7 Comparison between the simulated and measured true stress–strain data of the uniform ( a ) BCC and ( b ) SP lattices for different relative densities More
Image
Comparison of the data produced in this study with those in Ref. [ 29 ]. Sc...
Published Online: October 5, 2022
Fig. 8 Comparison of the data produced in this study with those in Ref. [ 29 ]. Scaling with relative density of ( a ) Young’s modulus, ( b ) yield strength, and ( c ) Poisson’s ratio. The yield strength was determined as 0.2% offset stress. Redrawn and adapted from Ref. [ 29 ]. More
Image
Image
Effect of the boundary conditions on the stress versus strain response for ...
Published Online: October 5, 2022
Fig. 10 Effect of the boundary conditions on the stress versus strain response for ( a ) BCC and ( b ) SP FGLs (Δ ρ = 0.3–0.7). CLF: constrained lateral faces; ULF: unconstrained lateral faces; and UBC: uniform boundary conditions. More
Image
Density-graded ( a ) and ( c ) BCC and ( b ) and ( d ) SP FGLs. Comparison ...
Published Online: October 5, 2022
Fig. 11 Density-graded ( a ) and ( c ) BCC and ( b ) and ( d ) SP FGLs. Comparison between experiments and predictions employing UBC with meshes of 12 × 12 × 12 elements. In ( a ) and ( b ) the FGLs are discretized by six layers (in the thickness direction) each having uniform material properties.... More
Image
Journal Articles
Journal Articles
Image
Schematic of synchrotron X-ray transmission experimental setup with sample ...
Published Online: September 23, 2022
Fig. 1 Schematic of synchrotron X-ray transmission experimental setup with sample geometry and schematic diffraction pattern. Only one sample is shown for simplicity, in practice, there were two samples placed face-to-face. R denotes the radial distance from the center of the Debye–Scherrer ring... More
Image
Integrated intensity for each pattern in one file. The frame with the highe...
Published Online: September 23, 2022
Fig. 2 Integrated intensity for each pattern in one file. The frame with the highest integrated intensity was then selected and used for strain calculations. More
Image
Image
X-ray diffraction lineout plots at the location of the TGO after ( a ), ( c...
Published Online: September 23, 2022
Fig. 4 X-ray diffraction lineout plots at the location of the TGO after ( a ), ( c ) 300 thermal cycles, and ( b ), ( d ) 600 thermal cycles. The insets of these lineout graphs indicate multiple α -Al 2 O 3 peaks used for the strain calculations. Peak integration was conducted every 10 deg aroun... More